The Miller Process for Refining Gold


Gold Bars   Agnico-Eagle


Ever wonder how most gold is refined?  No for the most part they don’t use the Wolhwill Process rather they use the Miller Process.  Unlike the Wolhwill Process described earlier in this series the Miller Process doesn’t use electricity but rather uses a stream of chlorine gas that is passed through a crucible of molten gold that produces gold that is 99.95 Fine.  It works to remove all the impurities because gold is least affected by chlorine so all the other impurities are removed as chloride slag floating on the surface of the molten gold where it is skimmed off.

In this process the dore bar is melted in an induction furnace where the chlorine gas is introduced into the molten metal by a rotating lance.  The lance is controlled in a very precise manner in a way there is no break through of the chlorine gas to the surface of the molten metal.  This removes what are termed “By-metals” like silver, copper, nickel along with any other metals.  The process also removes amphoteric elements like sulfur, selenium, tellurium, arsenic and bismuth.  These elements are all removed from the molten metal as chloride slag that floats to the surface of the charge where they are skimmed off for further treatment.

The process takes from 2 to 4 hours to complete with the chloride fumes being removed and filtered by a two stage wet filter or a two stage dry scrubbing system that maximizes the recovery of the chloride as well as the cleaning of the exhaust air from the process.  In the process slag is poured off the top of the melt into a crucible and allowed to slowly cool so any gold that has been caught up with the chlorides will settle to the bottom where it can be recovered as a button of gold when the crucible has cooled completely; it is then added to the remaining molten gold.  In this process the particles of gold remaining in the crucible are carefully removed by hand as well as the separation molds when they have cooled.

Once the gold has cooled it is poured through a ceramic filter directly into the granulation equipment or anode molds if the Wolhwill process is used to further refine the gold.

The main advantages of this process are its quick turnaround time, size of the charge that can be from 20 kg to as large as you like.  The rotating lances are made from temperature resisting ceramics for long life and evenly introduce chlorine to the melt.  The use of modern induction furnaces keep the consumption low using far less kilowatts then coil type furnaces for the same size of melted product.

In this process the gold produced is 99.95 Fine that is good enough for most commercial purposes.  Most of the metals remaining in the gold are mostly silver and copper that if desired can be removed using the Wolhwill Process producing gold bullion that is 99.999 Fine.   

3 comments:

  1. Thanks for always being the source that explains things instead of just putting an unjustified answer out there. I loved this post.
    refine palladium

    ReplyDelete
  2. Bullion Exchanges is a reputable Bullion Shop located in New York City's Diamond District.

    They have a wide variety of items such as, precious metals that range from the gold and silver to the prestigious platinum and palladium.

    They are offering an enormous range of products appealing to first time buyers and established collectors.

    ReplyDelete
  3. URGENT LOAN IS NOW AVAILABLE

    TODAY I GOT MY DESIRED LOAN AMOUNT $760K FROM A RELIABLE,TRUSTED AND REGISTERED PRIVATE LOAN COMPANY LAST WEEK,BUSINESS/HOME/COMPANY/PROJECT/PERSONAL LOAN? ARE NOW AFFORDABLE HERE FOR YOU TODAY CONTACT Call/Text +1(315)256-0479 Email profdorothyinvestment@gmail.com

    Hello, I'm here to testify of how i got my real estate business loan from PROF. MRS.DOROTHY JEAN INVESTMENTS (profdorothyinvestments@gmail.com) I don't know if you are in need of an urgent loan to pay bills, start business or build a house, they offer all kinds of loan Ranging from $5,000.00USD to $2,000,000.00USD with a low interest rate of 2% and loan duration of 1 to 33 years to pay back the loan secure and unsecured. Are you losing sleep at nights worrying how to get a Legit Loan Lender?
    MRS.DOROTHY JEAN holds all of the information about how to obtain money quickly and painlessly without cost/stress via Contacts Call/Text +1(315)256-0479
    Email profdorothyinvestment@gmail.com

    ReplyDelete